Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792-91 |
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene Mineral filled PP compound for interior automotive applications. Product meets GMP PP 056 and EBG-M4 D605-A specifications. Ash is 10%.Data provided by Multibase. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Plastcom SLOVALEN PH 96 FRD 1 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled Information provided by PolyPlastic Group. |
|||
Density | 0.992 - 1.44 g/cc | 0.0358 - 0.0520 lb/in³ | Average value: 1.21 g/cc Grade Count:211 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1413 Polyolefin TPO Granules, Dark Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1454 Polyolefin TPO Granules, Green Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1455 P Polyolefin TPO Granules, Black Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1459 Polyolefin TPO Granules, Azure Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID.. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E5S Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Borealis Daplen™ EE115AE TPO Compound Daplen EE115AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Density | 0.990 g/cc @Temperature 20.0 °C |
0.0358 lb/in³ @Temperature 68.0 °F |
|
Unipetrol R2 Heavy Fuel Oil Heavy fuel oil R2 is a mixture of mostly higher hydrocarbons obtained from crude oil through distillation and other refining processes. It may contain additives to lower its freezing point, or addit.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 3841 nat PA12 Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
BASF Diisopropanol-p-toluidine Formula: C13H21NO2CAS: 38668-48-3Description: Diisopropanol-p-toluidine is a colorless to yellowish paste with and amine-like odor. This product is only sparingly soluble in water.Synonyms: DIIPT, .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Tipco Tipcolene® HR 8240 - 10% Talc/Mineral Reinforced Impact Modified Polypropylene Copolymer, High Stiffness 10% Mineral Reinforced, High Stiffness, Impact Modified PP CopolymerApplications: Automotive ExteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |