Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works. |
|||
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Density | 0.985 - 0.995 g/cc | 0.0356 - 0.0359 lb/in³ | |
Solvay ANTAROX® LF 224 Surfactant Chemical Name: ETHOXYLATED PROPOXYLATED ISODECYL ALCOHOLS CAS: 37251-67-5; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX© LF-224 is used for t.. |
|||
Density | 0.985 g/cc | 0.0356 lb/in³ | Melt |
Covestro Desmopan® DP 9659DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
Density | 0.985 g/cc | 0.0356 lb/in³ | Melt |
Covestro Desmopan® DP 9662DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
Density | 0.985 g/cc | 0.0356 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Entira® ASSD100 Ionomer Resin DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets. Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LD.. |
|||
Density | 0.985 g/cc @Temperature 15.0 °C |
0.0356 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Solvesso™ 200 Aromatic Fluid Appearance: Transparent - Slight Yellow LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.985 g/cc | 0.0356 lb/in³ | |
BASF 2-Phenylethylamine Formula: C8H11NCAS: 64-04-0Description: 2-Phenylethylamine is a colorless to yellow liquid with an amine-like odor. Synonyms: Phenylethylamin, Benzolethanamin, PhenylethylamineApplications: Intermed.. |