Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
Nyco NYLITE® Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYLITE® Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3) is a natur.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
PolyOne OnFlex™ S EF 80A-3S1977 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Mytex Polymers AS66K-01 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792-91 |
Multibase Multi-Flex® TPO D-6206 This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems.Data provided by Multibase. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | |
Plastcom SLOVALEN PC 93 T 5 PP reinforced with 5% mineral filler Features: Modified PP for injection moulding with the content of 5% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packa.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 2781 |
Termopol Termoton® V5GA1090A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | |
Solvay ALKAMIDE® AJ58BN Surfactant Chemical Name: OLEIC ACID DIETHANOLAMIDEINCI NAME: Oleamide DEACAS: 93-83-4, 111-42-2, 67-56-1, 112-80-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMIDE AJ58.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Tipco Tipcolene® FPC 10 PPC - 10% Calcium Carbonate Reinforced Polypropylene Copolymer 10% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Tipco Tipcolene® FPZ-CL - 10% Talc/Mineral Reinforced Polypropylene Copolymer Compound 10% Mineral Reinforced PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183/A |
ExxonMobil Exxtral™ BMU130A Performance Polyolefin Product Description: Polyolefin injection molding compound with a good balance of stiffness, flow, and excellent processability for automotive bumper fascia and exterior trim applicationsAvailabilit.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Entec Hypro™ PPC-T10 Copolymer Polypropylene, 10% Talc Reinforced Information provided by Entec |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Diamond Polymers Softflex® SF 5060 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
Entec Hypro™ PPH-T10 Homopolymer Polypropylene, 10% Talc Reinforced Information provided by Entec |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D297 |
Dow Nordel® NDR 47130.01 EPDM Hydrocarbon Rubber Description: NDR 47130.01 is a very high molecular weight, semicrystalline EPDM grade with a fast cure rate. It also offers an excellent combination of:very fast mixing with good dispersion levelexc.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | |
BASF Pivaloyl Chloride Formula: C5H9ClOCAS: 3282-30-2Description Pivaloyl chloride is a colorless to light yellow liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Trimethylacetyl chloride, Neo.. |
|||
Density | 0.980 - 1.02 g/cc | 0.0354 - 0.0368 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 765A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | |
BASF Procom® X10S 773 Polypropylene Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
Lucobit Lucobit® 1218 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of special.. |
|||
Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |