Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
SABIC F01552 High Density Polyethylene for Blown Film Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-1052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 205W Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 205W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Total Lacqtene® 2004 TN 52 HDPE pipe
(discontinued **) LACQTENE® 2004 TN 52 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2004 TN 52 is best processed between 190 and 230°C.Informa.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7750 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM 5202LD HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good stiffnessExceptional processabilityGood ESCRApplications: Household & industrial chemical containersInformation provided by Chevron Phillips. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Microthene® F FA70000 High Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LB5604 High Density Polyethylene ApplicationsThe PETROTHENE LB 5604 series of polyethylene resins exhibits good stiffness and environmental stress cracking resistance. Typical applications include household chemical and person car.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 150-1498 HDPE Rotational Molding Resin Description: ICORENE 150-1498 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is.. |
|||
Density | 0.953 - 0.959 g/cc | 0.0344 - 0.0346 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4950 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) 5218EA High Density Polyethylene HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) BL4 HM 8255 High Density Polyethylene BL4 (HM 8255) is a high density polyethylene with Butene-1 as comonomer. It is a high molar mass, easily processable, high stiffness and impact good stress cracking resistance and even good molding .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® H5234 High Density Polyethylene ApplicationsALATHON H 5234 is a high flow injection molding grade of resin designed for fast cycle and thin wall molding. It provides cold temperature impact resistance. Typical applications inclu.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ISO 1183 |
Borealis Borstar® HE3476-LS Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Natural Gas Borstar HE3476-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® BB 38 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 210W Ethylene Vinyl Acetate DuPont™ Elvax® 210W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 240W Ethylene Vinyl Acetate DuPont™ Elvax® 240W is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 240W resins can be used for the following applications.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D 792 |
Total 5202 HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D 792 |
Total 5202LD HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
Density | 0.953 - 0.959 g/cc | 0.0344 - 0.0346 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DTDP Plasticizer Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-47-9Information provided by ExxonMobil |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Diamond Polymers NPP10-2528 Ethylene Vinyl Acetate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Arkema Group OREVAC® 9305 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM-D792 |
Braskem AD57 HDPE Monofilament Polyethylene Copolymer AD57 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process, designed for raffia extrusion, and Raschel knitted with excellent optical and mechanical propertie.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM-D792 |
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer GF4950HS resin is a high-density polyethylene (HDPE), bimodal copolymer offering a combination of good processability and environmental stress crack resistance (ESCR). It is thus recommended for the.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | Exxon Method |
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos J50-2000-119 HDPE HDPE J50-2000-119 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It i.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene HDPE 055952 features maximum toughness, good top loading capability, and high surface gloss. Applications include pails and beverage crates.Former A-Top Polymers product; part of Amco product line s.. |