Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Polymer Industries Densetec HMW Sheet Polymer Industries’ Densetec HMW is the extruded material needed when Densetec HDPE is not enough and Polyslick UHMW™ is not necessary. Densetec HMW has higher impact strength than HDPE and is mor.. |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4850B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, easy processing.Data provided by the manufacturer. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 56B4 HDPE Blow Molding Resin Extra-high stress crack resistance, Good processabilityApplications: Very high ESCR, Ideally suited for use in most food, pharmaceutical, households and industrial chemical applications, Little/no s.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Petromont 1202 High Density Polyethylene Resin Petromont HDPE 1202 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as shipping containers.. |
|||
Density | 0.946 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D4883 |
ExxonMobil HD 6605.29 Injection Molding Resin
(discontinued **) HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D792 |
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® MV-02520 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An experimental, very high flow, 20% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1475 |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.946 g/cc | 0.0342 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® ETP H4745 High Density Polyethylene ApplicationsALATHON H 4745 is a new, multi-purpose, high-flow resin featuring enhanced cold temperature impact performance, enhanced processability and thermal stability for fast cycling and exhibit.. |
|||
Density | 0.946 g/cc | 0.0342 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D4883 |
Ineos A4040 HDPE Ineos HDPE A4040 is a high density polyethylene copolymer produced using a supported catalyst process. It is a copolymer resin used mainly for the extrusion of crosslinked pipes according to the sil.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D4883 |
Ineos K44-11-128 HDPE Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.946 g/cc | 0.0342 lb/in³ | ISO 1183 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ISO 1183 |
Borealis FS1470 High Density Polyethylene FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D792-ISO 1183, ASTM D1505 |
DuPont Elvax® 350 Ethylene Vinyl Acetate DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: .. |
|||
Density | 0.946 g/cc | 0.0342 lb/in³ | ASTM D792 |
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6601.29 High Density Polyethylene Copolymer Resin Product Description: HD 6601 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance... |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 613 HPE Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable HDPE by gas injectionInformation provided .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
Axion Polymers Axpoly® HDPE12 1000 High Purity Molding Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin re.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM-D792 |
Braskem HE150 HDPE Monofilament Polyethylene Copolymer HE150 resin is a high-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It has been specially designed for the monofilament extrusion process and provides a good balan.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Westlake EMAC® Plus SP1330 22% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1330 is a 22% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1330 is.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D4883 |
ExxonMobil HD 8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |