Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.945 g/cc | 0.0341 lb/in³ | |
Pyrotek Pyroboard™ S1200 Roller Pyroboard™ S1200 is a long wearing durable, soft covering. It must be used in high heat areas in order for it to realize its full effectiveness. The heat helps to sinter the materials so that the.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ISO 1183-1 |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2209 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® CL-200YB (Black) Rotational molding crosslinkable high density polyethylene
(discont Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9396T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL4506 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Hexene CopolymerApplications: Multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containers (IBC)Formolene HL4506 is intended for large part blow molding appl.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D792 |
Global GA-3245 High Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsInformation provided by Global Polymers Corporation. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Reliance Industries Relene E41003 Polyethylene Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 297-285D High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 150-1499 HDPE Rotational Molding Resin Description: ICORENE 150-1499 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene EX1 (HF 7740F2) is high density polyethylene with Butene-1 as co monomer. It is a medium molecular mass with a narrow molar mass distribution.Application: stretched film tape used in manufacture o.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D792 |
Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D792 |
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2590 is a high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization is optimized .. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis HE3366 High Density Polyethylene HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer sk.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2202 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2202 is a 21.5% EMA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2202 provides exce.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2268 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2268 is a 24% EMA copolymer designed for extrusion coating, tie-layers, compounding, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D 792 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Density | 0.945 g/cc @Temperature 260 °C |
0.0341 lb/in³ @Temperature 500 °F |
Melt |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
Density | 0.945 g/cc @Temperature 15.6 °C |
0.0341 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exterex™ NP343 Synthetic Fluid Product Description: Esterex™ Polyol Esters are API category Group V fluids. Esterex™ Polyol Esters have excellent lower-temperature properties, good lubricating properties and low volatilities. E.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ASTM D4883 |
ExxonMobil HDPE BU46-060 High Density Polyethylene Resin Product Description: BU46-060 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ExxonMobil Method |
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate Product Description: Product Description: Optema TC 220 is an ethylene methyl acrylate copolymer, which can be used for making alloys, blends and compounds or be injection molded where softness and .. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Arkema Group OREVAC® 9318 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Density | 0.945 g/cc | 0.0341 lb/in³ | ISO 1183 |
Total Lacqtene® 2001 TN 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TN 46 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 TN 46 is used for sewage pipe, smooth protective condu.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Natural; ASTM D1505 |
Formosa Plastics Formolene® HP4306 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for l.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |