Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.933 - 0.937 g/cc | 0.0337 - 0.0339 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
DuPont Bynel® 3030 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA594189 is a pelletized LLDPE copolymer resin for injection molding thin-walled items requiring high flow and short cycle times. GA594189 exhibits excellent flow, warp resistance and sur.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA694189 is a pelletized LLDPE copolymer resin for injection molding. Typical applications include lids and thin-walled items that require high flow and short cycle times. GA694189 exhibi.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for extrusion and injection-blow molding. An antioxidant had been added to ensure thermal stability. Pro.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX5400 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1327 LMDPE Rotational Molding Resin Description: ICORENE 115-1327 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 324-1327 LMDPE Rotational Molding Resin Description: ICORENE 324-1327 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and me.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
Micropol Microlin ML21 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/2 Polyolefin Catalyst CT/2 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it all.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183/ISO 1872-2B |
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | Catalyst LE 4476; ASTM D792 |
Borealis Visico™/Ambicat™ LE4421/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4421 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | Catalyst LE 4476; ASTM D792 |
Borealis Visico™/Ambicat™ ME4425/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4476, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low .. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | with antiblock; ASTM D1505 |
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 701.ID Blown Film Resin Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | |
Dow Primacor® 3330 Ethylene Acrylic Acid (EAA) PRIMACOR® 3330 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent toughness, environmenta.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | |
Dow Primacor® 3340 Ethylene Acrylic Acid (EAA) PRIMACOR® 3340 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion and outstandin.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, Nor.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Density | 0.932 - 0.947 g/cc | 0.0337 - 0.0342 lb/in³ | Average value: 0.937 g/cc Grade Count:35 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |