Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® GI-2024-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: Granular; improved dispersion, easy processing, good ESCR.Applications: additives, masterbatches/compounding, housewares, trashcans, containers, toys.Data provid.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, High Gloss, Excellent ImpactUses: Large houseware containers, General purpose injection molding |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips 2151 High Impact, Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Medium Slip, High Antiblock, Low Blocking and Good Openability, Good ProcessabilityApplications:Trash bags and other linersProcessing Co.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
M. Holland Company LD225 LDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, High Clarity, High Gloss, Heat Sealable, Good Processability, Medium SlipUses: FilmProcessing Method: Blown FilmInformation pro.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | |
LyondellBasell Lupolen® 2425 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | |
LyondellBasell Lupolen® 2441 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D792 |
Micropol Microlin LL17 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® LL 2406 AA LLDPE Pipe Grade Applications:Drip irrigation pipeSmall potable water pipeInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
UBE F022SE Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Westlake Hifor Xtreme SC74849 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74849 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock, and polymer processing aid.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D-1505 |
Chevron Phillips MarFlex® 4571 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceHigh coefficient of friction Applications:.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade) Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 605BA Low Density Polyethylene Resin (European Grade) Product Description: LD 605BA is a general purpose LDPE grade, characterized by good stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Ant.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D4883 |
ExxonMobil LL 6100.17 Injection Molding Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE L L6101RQ Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | |
Arkema Group Evatane® 1006 VL 2E Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 200 at 210 µm for greenhouse coverage.ISO data provided by the.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | |
LyondellBasell Lupolen® 2424 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |