Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM112-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.980 g/cc | 0.0330 - 0.0354 lb/in³ | Average value: 0.945 g/cc Grade Count:71 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | Yield Density |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Density | 0.913 g/cc @Temperature 121 °C |
0.0330 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 1500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 613A Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade) Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D792 |
Dow ELITE™ 5500G Enhanced Polyethylene Resin ™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te.. |
|||
Density | 0.914 g/cc @Temperature 23.0 °C |
0.0330 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18360 Maleic Anhydride Modified Polyethylene OREVAC® 18360 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.914 g/cc @Temperature 0.000 °C |
0.0330 lb/in³ @Temperature 32.0 °F |
|
Akzo Nobel Trigonox® 121 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates.Information provided by Akzo Nobel Polymer Chemicals. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
BASF Lupragen® N 400 Trimethylamineoethylethanolamine Formula: C7H18N2OCAS: 2212-32-0Description: Trimethylaminoethylethanolamine is a colorless to light yellow liquid, with an amine-like odor. It is miscible with water and other organic solvents.Syno.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
ConocoPhillips 32 Spectrum Cutting Oil Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica.. |
|||
Density | 0.913 - 0.945 g/cc | 0.0330 - 0.0341 lb/in³ | Average value: 0.935 g/cc Grade Count:49 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |