Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 506P Polypropylene Homopolymer for Raffia Applications Product Description: PP 506P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speeds and low deniersLow tap.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 519A Polypropylene Homopolymer for Spunbond Applications Product Description: PP 519A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 519A has the following features:Consis.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 25-3701 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
Polymer Industries Densetec PP Homopolymer Sheet Polymer Industries’ Densetec Homopolymer Polypropylene exhibits the properties of high corrosion resistance, high temperature resistance, and great tensile strength. It maintains its stiffness at e.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Flint Hills P5L2Z-038 Random Copolymer Polypropylene Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene pro.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Borclear™ RF366MO Polypropylene Random Copolymer for Injection Molding Borclear™ RF366MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleati.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications Bormed RF825MO is a specially modified random copolymer polypropylene with high melt flow intended for use in medical and medical related articles. Bormed RF825MO is characterized by easy processab.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Borpact™ BC918CF Polypropylene Copolymer Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis HA104E Polypropylene Homopolymer HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis HC600TF Polypropylene HC600TF is a polypropylene homopolymer intended for thermoformed packaging applications. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPH 10042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPH 3051 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3051 is homopolymer.ApplicationATOFINA Polypropylene PPH 3051 is intended for the extrusion of flat bioriented films for food packaging or high strength adhesive tapes. Inf.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Total PPH 3825WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3825WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds.Antistat - FINA 3.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPH 5060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 5060 is homopolymer.ApplicationATOFINA Polypropylene PPH 5060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 5060 is.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPH 7069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Bormed™ RD808CF Polypropylene Random Copolymer Bormed™ RD808CF is a random copolymer. Applications: Bormed™ RD808CF is intended for packaging for medical devices, thin pouches, and packaging for pharmaceutical products. Additives: Bormed™ R.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis RD360MO Polypropylene Random Copolymer, Transparent RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM-D792 |
Braskem H 216 HOMO Polypropylene Homopolymer H 216 is a high melt flow rate homopolymer with narrow molecular weight distribution. It is designed for fiber extrusion processing with high toughness fibers. H 216 exhibits excellent processabilit.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792A |
Braskem H 504 XP Bioriented Film Polypropylene Description: H 504XP is a low melt flow rate homopolymer, designed specially for high speed lines of biorented films (BOPP). This product features a broad processing window with high output and regu.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792A |
Braskem H 605 Thermoforming Polypropylene Applications: Flat and corrugated sheets with high transparency; thermoformed packing with high transparency. Information provided by Braskem |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM-D792 |
Braskem H 611 HOMO Polypropylene Homopolymer H 611 is a low melt flow rate homopolymer that was specially designed for exposure to solar light. This product exhibits good processability and high melt resistance. It is designed for raffia extru.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Bapolene® PP5062 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin offers a superior balance of stiffness and impact strength. This product meets the FDA requirements of .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792A |
Braskem H 605 Extrusion Polypropylene Description: H 605 is a low melt flow rate homopolymer with high transparency. This resin is designed for extrusion and thermoforming. H 605 exhibits excellent processability, high output, excellent.. |