Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Network Polymers NPP 20-1001 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
PolyMirae Moplen HP600N Injection Molding Grade Polypropylene Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
LyondellBasell Pro-fax 6524 Polypropylene Homopolymer, Heat- and Extraction-Resistant Key Features: heat and extraction-resistant polypropylene homopolymer resin, FDA acceptable, high resistance to solventsApplications: appliances, automotive under-the-hood applicationsMeets FDA requ.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Key Features: high flow, compatible with hindered amine light stabilizers, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpageAppli.. |
|||
Density | >= 0.900 g/cc @Temperature 19.0 - 20.0 °C |
>= 0.0325 lb/in³ @Temperature 66.2 - 68.0 °F |
|
Kazanorgsintez H Waste Diesel Fuel Production Method: Waste diesel oil is produced when diesel oil is used a cracked gas cooling or flushing agent in the process of ethylene production. Application: Waste diesel oil is shipped to.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
M. Holland Company CP300 Polypropylene Copolymer Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Appliances, Business, Equipment, Tool/Tote Box, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformatio.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills AP5135-HS Impact Copolymer Polypropylene Medium impact copolymer, FDA compliantFeatures: Nucleated and heat stabilized.Applications: Injection molding: large, thin wall automotive interior parts and housewares.Former Huntsman polypropylene.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P4C4T-189 Polypropylene Homopolymer Features: Visbroken, Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: ClosuresInformation Provided by Flint Hills Resources |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P4C5B-075 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: tape extrusion and closures.Former Huntsman polypropylene products are now prod.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P4C5B-076 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: cutlery and closuresFormer Huntsman polypropylene products are now produced by .. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) C 30 S Polypropylene Polypropylene homopolymer with a good flow properties.Applications: film, yarn, monofilament, cast film and sheetsInformation provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EPD 60 R Polypropylene EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t.. |
|||
Density | 0.900 - 0.930 g/cc | 0.0325 - 0.0336 lb/in³ | TPI Method |
IRPC Polimaxx Polene PE300N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Mitsui ADMER® SE800 Elastomer Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Density | 0.900 g/cc @Temperature 15.6 °C |
0.0325 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 32 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® 1102L Homopolymer Polypropylene Homopolymer for Slit TapeFormolene® 1102L is a high molecular weight, highly isotactic, polypropylene homopolymer designed for extrusion processes, notably slit tape. It contains a unique combinati.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® 4101M Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101M is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6335N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and .. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
ExxonMobil PP4712E1 Polymer Grade for Oriented Film Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ExxonMobil Method |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ExxonMobil Method |
ExxonMobil PPT0170F Polypropylene Homopolymer Product Description: PPT0170F is an unstabilized homo polymer granular resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation prov.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Dow 6D43 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood spinning characteristicsComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW 6D43 Polypropylene Resin is intended for use in fiber spinning processes.Dow Announced.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Dow DS6D82 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D82 Polypropylene Resin is intended for use as a heat seal coati.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Dow R132-02A Polypropylene Random Copolymer Resin DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM C134 |
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Aclo Accucomp Polypropylene CPO406L Copolymer |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183/A |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |
|||
Density | 0.900 - 0.940 g/cc | 0.0325 - 0.0340 lb/in³ | Internal |
AKG Polymers Vision PP PPC BL3006 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |