Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.890 g/cc | 0.0322 lb/in³ | ISO 1183 |
Mytex Polymers AN18KW-01 FK Polypropylene, Rubber modified Description: Rubber modified polypropylene produced for automotive interior applications using Mytex® Technology. Specifically designed to achieve ductile performance at cold temperatures during a.. |
|||
Density | 0.890 - 1.21 g/cc | 0.0322 - 0.0437 lb/in³ | Average value: 1.06 g/cc Grade Count:130 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ISO 1183 |
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ISO 1183 |
LyondellBasell Adsylâ„¢ 5 X 37 F Polyolefin Description: Adsylâ„¢ 5 X 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a relatively high.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ASTM D792B |
LyondellBasell Astryn BA16G Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade polypropylene copolymer, good flexibility, high impact strength, good colorability, good processability, good weath.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | |
Silon Tabond 2002 Adhesive Resin TABOND 2002 is ethylene-octene Plastomer / LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 634 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Density | >= 0.890 g/cc | >= 0.0322 lb/in³ | |
Elastron® D SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureselectrical insulator with very low conductivityhas gra.. |
|||
Density | >= 0.890 g/cc | >= 0.0322 lb/in³ | |
Elastron® G SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 627 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 680 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.890 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil BB Mobil DTE Oil Double Letter Series The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing.. |
|||
Density | 0.890 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | |
ConocoPhillips Hydroclear® 320 Circulating Oil Description: Conoco Hydroclear Circulating Oil is a high-quality, rust-inhibited circulating oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Circulating Oil is specially form.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | DIN 51757 |
BASF Butylethanolamine Formula: C6H15NOCAS: 111-75-1Information provided by BASF |
|||
Density | 0.892 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 40 1640 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.892 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 40 1640 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |