Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 11M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 5W-50 Mobil 1 5W-50 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils.. Mobil 1 5W-50 is engineered to help keep en.. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 75W-90 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Density | 0.859 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Syncon® 460 Synthetic EP Gear Oil, AGMA No. 7EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Density | 0.857 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Density | 0.857 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 11M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 5W-50 Mobil 1 5W-50 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils.. Mobil 1 5W-50 is engineered to help keep en.. |
|||
Density | 0.857 g/cc | 0.0310 lb/in³ | ASTM D792 |
Dow Engage® 8842 Polyolefin Elastomer Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle si.. |
|||
Density | 0.857 - 0.913 g/cc | 0.0310 - 0.0330 lb/in³ | ASTM D792 |
Dow Engage® Polyolefin Elastomer Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. .. |
|||
Density | 0.858 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Hydroclear® 150 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.858 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Hydroclear® 22 Quench Oil Description: Conoco Hydroclear® Quench Oil is a high-quality metal heat-treating and quenching oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Quench Oil is specially formul.. |
|||
Density | 0.857 g/cc | 0.0310 lb/in³ | |
ConocoPhillips MV32 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Density | 0.859 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Hydroclear® 32 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.858 g/cc | 0.0310 lb/in³ | |
ConocoPhillips Hydroclear® 32 TCS Slideway lubricant Description: Conoco Hydroclear® TCS Slideway Lubricant is a premium demulsible machine tool way lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear TCS Slideway Lubricant .. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 75W-90 Gear Lubricant LS Mobil 1 Synthetic Gear Lubricant LS is a supreme performance, synthetic, multi-purpose, SAE 75W-90 automotive gear lubricant designed to meet the highest level performance requirements of modern pas.. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 75W-90 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Density | 0.859 g/cc @Temperature 15.0 °C |
0.0310 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 75W-90 Gear Lubricant LS Mobil 1 Synthetic Gear Lubricant LS is a supreme performance, synthetic, multi-purpose, SAE 75W-90 automotive gear lubricant designed to meet the highest level performance requirements of modern pas.. |