Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.828 - 0.871 g/cc @Temperature 15.0 °C |
0.0299 - 0.0315 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Light Stabilized Oil Hydrogenate Stabilized oil hydrogenates are a fraction boiling above approximately 250°C, obtained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of.. |
|||
Density | 0.829 - 0.834 g/cc | 0.0299 - 0.0301 lb/in³ | ASTM D4052 |
ExxonMobil EXXAL® 8 Isooctyl Alcohol CAS Number: 68526-83-0EINECS Number: 2712314Information provided by ExxonMobil |
|||
Density | 0.827 g/cc @Temperature 15.6 °C |
0.0299 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D130 Dearomatized Fluid Availability: Asia Pacific, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.827 g/cc @Temperature 15.6 °C |
0.0299 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn™ 6 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Density | 0.827 g/cc @Temperature 15.6 °C |
0.0299 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn Plus™ 6 Advanced Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices.. |
|||
Density | 0.827 g/cc | 0.0299 lb/in³ | |
3M 80 Rubber and Vinyl Spray Adhesive A high performance neoprene based contact aerosol spray adhesive.Features:It is typically used to bond rubber, supported vinyl, leather, wood, metal and many plasticsProvides exceptional heat resist.. |
|||
Density | 0.827 g/cc | 0.0299 lb/in³ | |
BASF Octamethylenediamine Formula: C8H20N20CAS: 373-44-4Description: Octamethylenediamine is a colorless solidified mass with an amine-like odor. It is miscible with water.Synonyms: 1,8-DiamineoctaneApplications: It is used.. |
|||
Density | 0.827 g/cc | 0.0299 lb/in³ | |
3M Scotch-Weld™ Foam Fast 74 Adhesive An extremely fast tacking industrial grade spry adhesive for bonding foam and fabricFeatures:Used for bonding flexible urethane or latex foam together and to other materials such as wood, metal and .. |
|||
Density | 0.827 g/cc | 0.0299 lb/in³ | |
3M Scotch-Weld™ Hi-Strength Laminating 92 Spray Adhesive A high performance, high temperature resistant, tack industrial grade spray adhesive designed for use in a wide variety of applications.Features:It can be used for high pressure laminate, veneers, f.. |