Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.820 - 0.880 g/cc | 0.0296 - 0.0318 lb/in³ | fired density (compressed) |
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Density | 0.820 - 0.880 g/cc | 0.0296 - 0.0318 lb/in³ | fired density (compressed) |
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Density | 0.820 - 4.20 g/cc | 0.0296 - 0.152 lb/in³ | Average value: 1.29 g/cc Grade Count:210 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Density | 0.820 - 0.820 g/cc @Temperature 240 - 240 °C |
0.0296 - 0.0296 lb/in³ @Temperature 464 - 464 °F |
Average value: 0.820 g/cc Grade Count:1 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 0.820 - 11.0 g/cc | 0.0296 - 0.397 lb/in³ | Average value: 1.42 g/cc Grade Count:484 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Density | >= 0.820 g/cc @Temperature 20.0 °C |
>= 0.0296 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-12 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM D1475-85 |
Lord Adhesives Aeroglaze® 9953 Epoxy Primer Thinner Aeroglaze® 9953 thinner is used to reduce Aeroglaze epoxy viscosity for spray applicationsAll information provided by Lord. |
|||
Density | 0.820 - 0.845 g/cc @Temperature 15.0 °C |
0.0296 - 0.0305 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Grade B Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |
|||
Density | 0.820 - 0.845 g/cc @Temperature 15.0 °C |
0.0296 - 0.0305 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Grade D Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22 Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen.. |
|||
Density | 0.818 g/cc @Temperature 15.0 °C |
0.0296 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D100 Dearomatized Fluid Availability: Africa & Middle East, Europe and South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | Calculated number using basis weight and thickness |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | Calculated number using basis weight and thickness |
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Density | 0.820 g/cc @Temperature 15.6 °C |
0.0296 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices.. |
|||
Density | 0.820 g/cc @Temperature 15.6 °C |
0.0296 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM C134 |
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM C134 |
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Density | 0.819 g/cc | 0.0296 lb/in³ | |
BASF 2-(Diethylamino)ethylamine Formula: C6H16N2CAS: 100-36-7Description: 2-(Diethylamino)ethylamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: N,N-Diethyl-1,2-ethanediamine, 2-(Di.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
BASF N-Ethylpiperidine Formula: C7H13NCAS: 766-09-6Description: N-Ethylpiperidine is a colorless to yellow liquid, with an amine-like odor characteristic with this product. It is miscible with water.Synonyms: EPIP, 1-Eth.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | Sintered; ASTM D792 |
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire.. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
3M 4411B Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
3M 4411G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
3M 4411N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Density | 0.820 g/cc | 0.0296 lb/in³ | |
3M 4412N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Density | 0.820 - 0.845 g/cc @Temperature 15.0 °C |
0.0296 - 0.0305 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Grade F Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |