Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.789 - 0.791 g/cc | 0.0285 - 0.0286 lb/in³ | Premium Grade, 1st Grade |
Kazanorgsintez Acetone, Commercial Production Method: Composition is produced by the cumene method. Application: The product is used for the synthesis of acetic anhydride, acetone cyanohydrine, diphenyl propane and other organic .. |
|||
Density | 0.788 g/cc @Temperature 20.0 °C |
0.0285 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell ARCOPURE® High Purity MTBE, Methyl tertiary butyl ether Information provided by Lyondell. |
|||
Density | 0.788 g/cc @Temperature 20.0 °C |
0.0285 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell Ethanol, 200 Proof Information provided by Lyondell. |
|||
Density | 0.790 - 0.830 g/cc | 0.0285 - 0.0300 lb/in³ | RP-17617 |
Solvay RHODOLINE® 581B Surfactant Description: Mineral oil defoamers for high PVC systems Chemical Name: DEFOAMERCAS: 64742-47-8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility(2% in DI Water): Coarse Di.. |
|||
Density | 0.788 g/cc @Temperature 15.0 °C |
0.0285 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Isopar™ N Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu.. |
|||
Density | 0.790 g/cc | 0.0285 lb/in³ | |
3M Scotch-Weld™ AC452 Instant Adhesive Activator 3M™ Scotch-Weld™ Instant Adhesive Activator AC452 is acetone based and will attack some plastics.Information provided by 3M |
|||
Density | 0.790 g/cc | 0.0285 lb/in³ | |
3M Scotch-Weld™ AC79 Instant Adhesive Primer 3M™ Scotch-Weld™ Instant Adhesive Primer AC79 is a California compliant version of AC78.Information provided by 3M |
|||
Density | >= 0.790 g/cc | >= 0.0285 lb/in³ | |
3M Scotch-Weld™ MG79 AC Medical Grade Instant Adhesive Primer 3M™ Scotch-Weld™ Medical Grade Instant Adhesive Primers are liquid chemical products used in conjunction with 3M™ Scotch-Weld™ Medical Grade Instant Adhesives. MG 79 AC is a cyanoacrylate primer.. |
|||
Density | 0.790 g/cc | 0.0285 lb/in³ | |
3M Scotch-Weld™ 3989 Anaerobic Adhesive Activators 3M™ Scotch-Weld™ Anaerobic Activators are general-purpose surface activators/primers that cure anaerobic adhesives or inactive or very cold surfaces. For normal active surfaces, 3M™ Scotch-Weld™.. |
|||
Density | 0.790 g/cc | 0.0285 lb/in³ | |
3M Scotch-Weld™ AC12 Instant Adhesive Activator 3M™ Scotch-Weld™ Instant Adhesive Activator AC12 is isopropyl alcohol basedInformation provided by 3M |
|||
Density | 0.790 g/cc | 0.0285 lb/in³ | |
3M Scotch-Weld™ AC649 Anaerobic Adhesive Activators 3M™ Scotch-Weld™ Anaerobic Activators are general-purpose surface activators/primers that cure anaerobic adhesives or inactive or very cold surfaces. For normal active surfaces, 3M™ Scotch-Weld™.. |