Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.774 g/cc | 0.0280 lb/in³ | |
Pyrotek T-20 Fiberglass Fabric Close woven fiberglass. Does not cause severe skin irritation. Lightweight, light-brown, chemical resistant fabric.Information provided by Pyrotek. |
|||
Density | 0.775 - 1.28 g/cc | 0.0280 - 0.0462 lb/in³ | Average value: 1.06 g/cc Grade Count:25 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Density | 0.775 - 0.840 g/cc | 0.0280 - 0.0303 lb/in³ | |
Unipetrol JET A-1 AFQRJOS Issue 18 Jet Kerosene Jet Kerosene is a mixture of liquid hydrocarbons, with boiling point ranging between 135 and 280°C. It is obtained from crude oil by distillation and by other technological processes. It may contai.. |
|||
Density | 0.775 g/cc @Temperature 15.6 °C |
0.0280 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D3135 Naphtha Dearomatized Fluid Availability: North America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.775 g/cc @Temperature 15.0 °C |
0.0280 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D40 Dearomatized Fluid Availability: Africa & Middle East, Asia Pacific, Europe, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.774 g/cc @Temperature 15.0 °C |
0.0280 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Varsol™ 30 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |