Polymer Property : Density = 0.0238 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.660 g/cc
0.0238 lb/in³
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Density 0.660 - 0.700 g/cc
0.0238 - 0.0253 lb/in³
Unipetrol C5 Fraction
C5 fraction is mixture of mainly alifatic and cyclic hydrocarbons C5. It is colourless, volatile, extremely combustible and easily inflammable liquid with characteristic odour. It generates as a by-..