Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.631 g/cc @Temperature 15.0 °C |
0.0228 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ Pentane 100 S Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.631 g/cc @Temperature 15.0 °C |
0.0228 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ Pentane 80 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.630 - 0.770 g/cc | 0.0228 - 0.0278 lb/in³ | ISO 845-88 |
Eurofoam Gummicell GU 250 0,70 NR Foam Natural rubber foam. Uses: industrial purposes, ceramics, mouse pads, diecutting, eletronics, and electromechanicsInformation provided by Eurofoam s.r.l. |
|||
Density | 0.630 g/cc | 0.0228 lb/in³ | |
BASF Trimethylamine Anhydrous Formula: C3H9NCAS: 57-50-3Description Trimethylamine anhydrous is a colorless gas that can also be liquefied, and has an amine-like odor. It is fully soluble with water.Synonyms: TMA, N,N-Dimethylm.. |