Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1016A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1016A / 5 phr S1.. |
|||
Density | 0.529 - 0.560 g/cc | 0.0191 - 0.0202 lb/in³ | Dried |
Pyrotek Pyrocast L-40 Insulating Refractory Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C.. |
|||
Density | 0.530 - 0.570 g/cc | 0.0191 - 0.0206 lb/in³ | Free flowing, Typical |
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Density | 0.529 g/cc | 0.0191 lb/in³ | Nominal |
Unifrax Fiberfrax® High Density Rope Fiberfrax textile products are durable, high temperature, ceramic fiber packing materials that are well-suited for industrial applications. They are noted for their superior insulating and sealing .. |
|||
Density | 0.529 g/cc | 0.0191 lb/in³ | Nominal |
Unifrax Fiberfrax® Round Braid Fiberfrax textile products are durable, high temperature, ceramic fiber packing materials that are well-suited for industrial applications. They are noted for their superior insulating and sealing .. |
|||
Density | 0.529 g/cc | 0.0191 lb/in³ | ASTM C134 |
BNZ Materials BNZ-23A Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1027A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Oven Aging, measured on a 100 phr S1027A / 20 phr V0022G system. Deformation, Hot .. |
|||
Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1075A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1074A / 5 phr S1.. |