Density 0.500 g/cc
0.0181 lb/in³
Average Density
Potters Industries Conduct-O-Fil® SH230S33 Silver-Coated Hollow Glass Spheres
Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include conductive paints and coatings, aerospac..
Density 0.500 - 1.20 g/cc
0.0181 - 0.0434 lb/in³
Average value: 1.03 g/cc Grade Count:48
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..
Density 0.500 - 1.20 g/cc
0.0181 - 0.0433 lb/in³
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
Description: Indium oxide doped with tin oxide, ITO, is used to make transparent conductive coatings. Thin film layers can be deposited by electron-beam evaporation or sputtering. Roll or web coatin..
Density 0.500 g/cc
0.0181 lb/in³
MarkeTech H-2 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
Density 0.500 g/cc
0.0181 lb/in³
Cured
ITW Plexus Plexusâ„¢ MA200 Methacrylate Adhesive
Two component adhesive that expands to twice original volume without toxic blowing agents. Used where weight, gap-filling, or increased toughness (vibration damping) is requires for the bonded join..
Density 0.500 g/cc
0.0181 lb/in³
Solvay MACKOLA® CAS-100N Surfactant
Product Description: Mackol CAS-100N is sodium coco-sulfate derived from natural coconut oil. In the needle form, the product is free flowing and disperses easily in water. Heat is required to fully..
Density 0.500 g/cc
0.0181 lb/in³
Solvay RHODAQUAT® M-242B/99 Surfactant
Description: Rhodaquat® M-242B/99 is high purity cationic surfactant A free flowing crystalline powder has unique property of static and tangling elimination, imparting soft and elegant feel to h..
Density 0.500 g/cc
0.0181 lb/in³
ASTM D792
Covestro Baydur® STR/F-275 IMR Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System
Contains continuous strand fiberglass mat.0.0985 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer..
Density 0.500 g/cc
0.0181 lb/in³
helium pycnometer
CRG Industries Advantic™ 30 Syntactic Foam
Advantic is a series of lightweight, engineered foams consisting of manufactured glass, polymer, or ceramic hollow spheres embedded in a resin matrix, such as epoxy or cyanate ester. CRG Industries’..
Density 0.500 - 0.600 g/cc
0.0181 - 0.0217 lb/in³
BASF Imidazole
Formula: C3H4N2CAS: 288-32-4Description: Imidazole is a crystalline powder with an amine-like odor. It is soluble in water.Synonyms: 1,3-Diaza-2,4-cyclopentadiene, 1,3-Diazole, Imidazol, Methanimid..
Density 0.500 g/cc
0.0181 lb/in³
Typical, 3M QCM 14.24.6
3M H50/10000EPX Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.500 g/cc
0.0181 lb/in³
Geon® 1169; Internal Method
PolyOne Syncure™ S1054A Polyethylene, Crosslinked (XLPE)
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Oven Aging, Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1054..
Density 0.500 g/cc
0.0181 lb/in³
Geon® 1169; Internal Method
PolyOne Syncure™ S1060A Polyethylene, Crosslinked (XLPE)
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1060A / 5 phr S1..
Density 0.500 g/cc
0.0181 lb/in³
BASF 2-Butyne-1,4-diol Pure Cryst.
Formula: C6H15NOCAS: 110-65-6Description: N-Butyldiethanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportionsSynonyms: BDEA, N-Butyldiethanol..
Density 0.500 g/cc
0.0181 lb/in³
Zelfo Technology Zelfo® HG Cellulose Fiber Material
Zelfo® is a high performance bio-based material. Patented fibre technology developed by Zelfo Technology transforms 100% renewable or recycled cellulose fibres and water into self-binding Zelfo mat..
Copyright © lookpolymers.com All Rights Reserved