Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.471 g/cc | 0.0170 lb/in³ | ASTM D3574 |
Saint-Gobain COHRlastic® R10460 Medium Flame Retardant Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Density | 0.471 g/cc | 0.0170 lb/in³ | ASTM D3574 |
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Density | 0.471 g/cc | 0.0170 lb/in³ | ASTM D3574 |
Saint-Gobain COHRlastic® R10480 Medium Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Density | 0.471 g/cc | 0.0170 lb/in³ | ASTM D1667 |
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Density | 0.471 g/cc | 0.0170 lb/in³ | ASTM D1667 |
Saint-Gobain Normount® V4600 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive Description: Ideal for Exterior Mounting Applications: Normount® V2800/V4600 closed-cell foam bonding tapes are highly conformable. The foam substrate allows energy and stress in the joint to be .. |
|||
Density | 0.471 g/cc | 0.0170 lb/in³ | ASTM D1667 |
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive Description: Ideal for Exterior Mounting Applications: Normount® V2800/V4600 closed-cell foam bonding tapes are highly conformable. The foam substrate allows energy and stress in the joint to be .. |