Density 0.420 g/cc
0.0152 lb/in³
Effective density of spheres
Potters Industries Q-Cel® 6042S
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Density 0.420 g/cc
0.0152 lb/in³
3M Cushion-Mount™ 1920S Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Density 0.420 g/cc
0.0152 lb/in³
Typical, 3M QCM 14.24.6
3M HGS8000X Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.420 g/cc
0.0152 lb/in³
3M S42XHS Glass Bubbles
3M™ Glass Bubbles S42XHS are high-strength additives for polymers made from a water-resistant and chemically stable sodalime-borosilicate glass. These hollow glass microspheres can be compounded wi..
Density 0.420 g/cc
0.0152 lb/in³
apparent nominal; ASTM C271
3A Composites Core Materials AIREX® PXc.420 Fiber-Reinforced Structural Foam
AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu..
Density 0.420 g/cc
0.0152 lb/in³
apparent nominal; ASTM C271
3A Composites Core Materials AIREX® PXw.420 Fiber-Reinforced Structural Foam Panel
AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou..
Density 0.420 g/cc
0.0152 lb/in³
3M Cushion-Mount™ 1915M Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Density 0.420 g/cc
0.0152 lb/in³
3M Cushion-Mount™ 1920M Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..