Physical Properties Metric English Comments
Density 0.368 g/cc
0.0133 lb/in³
ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.368 g/cc

@Temperature 121 °C
0.0133 lb/in³

@Temperature 250 °F
Dry Density
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M22 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 0.368 g/cc

@Temperature 121 °C
0.0133 lb/in³

@Temperature 250 °F
Dry Density
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M607 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 0.368 - 0.481 g/cc

@Treatment Temp. 982 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 1800 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® Isofoam® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..
Density 0.368 - 0.481 g/cc

@Treatment Temp. 982 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 1800 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..
Density 0.368 - 0.481 g/cc

@Treatment Temp. 1260 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 2300 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® RG Plus Insulation
Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process..