Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.270 g/cc | 0.00975 lb/in³ | Effective Density as measured by liquid displacement |
Potters Industries Q-Cel® 7028 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Density | 0.270 g/cc | 0.00975 lb/in³ | Solid |
Sawbones Fourth-Generation Simulated Cancellous Bone (Rigid Polyurethane Bone) Fourth-generation bones model natural cortical bone using a mixture of short glass fibers and epoxy resin pressure injected around a foam core. Standard bone models are manufactured with a solid rig.. |
|||
Density | 0.270 g/cc | 0.00975 lb/in³ | |
Sawbones Second-Generation Simulated Cancellous Bone (Solid) Rigid Polyurethane BoneSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous ma.. |
|||
Density | 0.270 g/cc | 0.00975 lb/in³ | |
Sawbones Third-Generation Simulated Cancellous Bone (Solid) Rigid Polyurethane BoneSawbones® standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid.. |
|||
Density | 0.270 g/cc | 0.00975 lb/in³ | Foam |
Aptek DI-STRATE 1500-1 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Iridium Satellite AntennasInformation provi.. |
|||
Density | 0.270 - 1.71 g/cc | 0.00975 - 0.0618 lb/in³ | Average value: 0.767 g/cc Grade Count:9 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |