Physical Properties Metric English Comments
Density 0.190 g/cc
0.00686 lb/in³
Effective density of spheres
Potters Industries Q-Cel® 5019
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Density 0.190 g/cc
0.00686 lb/in³
Effective density of spheres
Potters Industries Q-Cel® 6019
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Density 0.190 g/cc
0.00686 lb/in³
Effective Density as measured by liquid displacement
Potters Industries Q-Cel® 6019S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Density 0.190 g/cc
0.00686 lb/in³
Effective Density as measured by liquid displacement
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Density 0.190 g/cc
0.00686 lb/in³
Pyrotek Jacketed mesh core Tadpoles
304 stainless steel mesh core with continuous fiberglass jacket. Excellent where no mounting flange is required.AdvantagesGood Abrasion Resistance Excellent Compression and Recall Information provi..
Density 0.190 - 4.80 g/cc
0.00686 - 0.173 lb/in³
Average value: 1.49 g/cc Grade Count:273
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Density 0.190 g/cc
0.00686 lb/in³
Pour Density
TIMCAL ENSACO™ 150G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Density 0.190 - 0.250 g/cc
0.00686 - 0.00903 lb/in³
3M S22 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.190 g/cc
0.00686 lb/in³
Pyrotek Mesh core / V-5 Tadpoles
Inconel mesh core with jacket and mounting flange consisting of high-temperature, ceramic fiber.AdvantagesFair Abrasion Resistance Excellent Compression and Recall Information provided by Pyrotek.
Density 0.190 g/cc
0.00686 lb/in³
Pyrotek Mesh core / Z-6W Tadpoles
304 stainless steel mesh core with jacket and mounting flange consisting of wire reinforced, densely woven glass cloth.AdvantagesExcellent Abrasion Resistance Excellent Compression and Recall Inform..
Copyright © lookpolymers.com All Rights Reserved