Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek L-8 Fiberseal Blanket Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek L8 Fiber Seal Pre-cut Gasket A lightweight needled blanket which is strong and durable.Information provided by Pyrotek. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek M-8 Fiber Seal Pre-cut Gasket Contains no binders and is not changed by exposure to high temperatures.Information provided by Pyrotek. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Sharadaa Ceramics And Bulk Fiber Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Sharadaa Ceramics Blankets Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Zircar Refractory Composites RSBL-SOL8 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Density | 0.128 - 0.176 g/cc | 0.00462 - 0.00636 lb/in³ | |
3M Balsa Panels 3M™ Balsa Panels are made of end grain balsa, a highly processed ultra light wood product, imparts impressive strength and stiffness to the sandwich panel. The end grain confiation of balsa provide.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek M-8 Fiberseal Blanket Stitched with high-temperature fibers. Contains no binders. Not changed by exposure to high temperatures.Dimensions610 mm x 7.6 m25 mm thickApplicationsHigh-temperature gaskets Furnace linings Gen.. |