Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.112 g/cc | 0.00405 lb/in³ | Typical Compression Density |
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | Compressed Density |
Northstar Polymers MPP-R07B Polyurethane Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-.. |
|||
Density | >= 0.112 g/cc | >= 0.00405 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ C41NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.112 - 0.176 g/cc | 0.00405 - 0.00637 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | |
Unifrax Fiberfrax® HSA (OF) Ceramic Fiber Paper HSA paper is made from high surface area (HSA) fibers that contain a low percentage of unfiberized material. Use of this fiber results in a paper with lighter weight and extremely low thermal condu.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | |
Unifrax Fiberwall® Bonded 22 Bonded Module System Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | |
Unifrax Fiberwall® Bonded 30 Bonded Module System Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/8 - 7.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | |
Hexcel® HexWeb® HRP - 3/16 - 7.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | |
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.112 g/cc | 0.00405 lb/in³ | Molded density, ASTM D1622 |
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.112 - 0.122 g/cc | 0.00405 - 0.00441 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |