Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0913 g/cc | 0.00330 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 3/16-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0913 g/cc | 0.00330 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 3/16-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0913 g/cc | 0.00330 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Density | 0.0913 g/cc | 0.00330 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 3/16-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Density | 0.0913 g/cc | 0.00330 lb/in³ | |
Lendell Medisponge® Latex FreeThis line of foam is specifically directed towards the medical industry. This line has regulatory approval under FDA Guidelines 10993-1.Applications:Surgeons Blankets, Swabs, Wraps, Wipe.. |