Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0250 g/cc | >= 0.000903 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0250 - 0.100 g/cc | 0.000903 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | >= 0.0250 g/cc | >= 0.000903 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 170R Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0250 - 0.100 g/cc | 0.000903 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 170R Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | >= 0.0250 g/cc | >= 0.000903 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 270R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0250 - 0.100 g/cc | 0.000903 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 270R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0250 g/cc | >= 0.000903 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Styrocell® D833A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |
|||
Density | 0.0250 g/cc | 0.000903 lb/in³ | 77 second cycle time |
Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding 100% PolystyrenePre-expansionThis is the low pentane version for high quality block molding.Block MouldingJackocell® S2314 represents the favorite choice for the manufacture of high quality insul.. |
|||
Density | 0.0250 g/cc | 0.000903 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0250 - 0.0350 g/cc | 0.000903 - 0.00126 lb/in³ | sheet density |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0250 - 0.0330 g/cc | 0.000903 - 0.00119 lb/in³ | sheet density |
Zotefoams Plastazote® LD28 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0250 - 0.0330 g/cc | 0.000903 - 0.00119 lb/in³ | sheet density |
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0250 - 0.0300 g/cc | 0.000903 - 0.00108 lb/in³ | ISO 845-88 |
Eurofoam Euroflex Art. 110 Polyurethane Foam Information provided by Eurofoam s.r.l. |
|||
Density | 0.0250 g/cc | 0.000903 lb/in³ | |
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 551 DU 20 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 551 WU 20 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 820 SL 40 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 820 SL 80 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 820 SLU 40 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 820 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0250 g/cc | 0.000903 lb/in³ | ISO 845 |
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Density | <= 0.0250 g/cc | <= 0.000903 lb/in³ | TMA |
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0250 - 1.39 g/cc | 0.000903 - 0.0504 lb/in³ | Average value: 0.407 g/cc Grade Count:149 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |