Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0220 - 0.0350 g/cc | 0.000795 - 0.00126 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV.. |
|||
Density | 0.0220 - 0.0500 g/cc | 0.000795 - 0.00181 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 35B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preforms for the "lost foam" casting technique used in foundries.Information provided by NO.. |
|||
Density | 0.0220 - 0.0800 g/cc | 0.000795 - 0.00289 lb/in³ | |
Polimeri Europa Extir® EH 2000 Expandable Polystyrene Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use.. |
|||
Density | 0.0220 - 0.0600 g/cc | 0.000795 - 0.00217 lb/in³ | |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |
|||
Density | 0.0220 - 0.0600 g/cc | 0.000795 - 0.00217 lb/in³ | Density range normally used |
Polimeri Europa Extir® P 1212 Expandable Polystyrene, Special Purpose
(discontinued **) Particle size range is 0.2 - 0.5 mm. Minimum apparent density on a discontinuous pre-expander is 21 g/l. Minimum apparent density on a continuous pre-expander is 25 g/l.Processing technology used .. |
|||
Density | 0.0220 - 0.0500 g/cc | 0.000795 - 0.00181 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 522 FC Expandable Polystyrene TPC - 522 FCApplications: shape molding with wall thickness |
|||
Density | 0.0220 - 0.0500 g/cc | 0.000795 - 0.00181 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 526 WP Expandable Polystyrene TPC - 526 WPApplications: very thin-wall water proof shape molding products with wall thickness |
|||
Density | 0.0220 g/cc | 0.000795 lb/in³ | 2.5 minute residence time |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |
|||
Density | 0.0220 - 0.0280 g/cc | 0.000795 - 0.00101 lb/in³ | |
Akzo Nobel Expancel® 461 DE 40 d25 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0220 - 0.0280 g/cc | 0.000795 - 0.00101 lb/in³ | |
Akzo Nobel Expancel® 461 DET 40 d25 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | >= 0.0220 g/cc | >= 0.000795 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Styrocell® D733A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol.. |