Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 140R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 150F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 150F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 250R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 34RC Regular Expandable Polystyrene Applications: PackagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 35MB Modified Expandable Polystyrene Applications: Fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 35MC Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Batch Expansion |
NOVA Chemicals EPS M97C Expandable Polystyrene Resin Applications Insulation, SIP's, ICF's, Fabricated PackagingInformation provided by NOVA Chemicals |
|||
Density | 0.0200 - 0.0350 g/cc | 0.000723 - 0.00126 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 35C Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV.. |
|||
Density | 0.0200 - 0.0800 g/cc | 0.000723 - 0.00289 lb/in³ | |
Polimeri Europa Extir® EH 3000 Expandable Polystyrene Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Density | 0.0200 - 0.0550 g/cc | 0.000723 - 0.00199 lb/in³ | |
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene
(discontinued **) Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Density range normally used |
Polimeri Europa Extir® C 2000 Expandable Polystyrene, Fast Molding
(discontinued **) Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type C 2000 is: Molding, Vacuum.Specific characteristics: Ver.. |
|||
Density | 0.0200 - 0.0350 g/cc | 0.000723 - 0.00126 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 422 FC Expandable Polystyrene TPC - 422 FCApplications: shape molding of 6-10mm wall thicknessInformation provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.0200 - 0.0270 g/cc | 0.000723 - 0.000975 lb/in³ | sheet density |
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | ISO 845-88 |
Eurofoam Polycell PE 30 Polyethylene Foam Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | |
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | ISO 845 |
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | ISO 845 |
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | 105 second cycle |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Normal molded density |
NOVA Chemicals Styrocell® D733A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol.. |
|||
Density | 0.0200 - 0.0350 g/cc | 0.000723 - 0.00126 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 426 WP Expandable Polystyrene TPC - 426 WPApplications: very low water absorption, cycling shape molding of 6-10 mm wall thicknessInformation provided by Iran Petrochemical Commercial Co. |