Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.00545 - 1.88 g/cc | 0.000197 - 0.0679 lb/in³ | Average value: 1.35 g/cc Grade Count:132 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |