Polymer Property : Density = 4.40 g/cc
Polymer Property :
Density =
4.40 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 518.001 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 518.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 518.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 526.062 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 526.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 526.077 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 526.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 560.077 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only
Density
3.80
-
4.40
g/cc
0.137
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 518.054 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density
3.70
-
4.40
g/cc
0.134
-
0.159
lb/in³
ASTM B417
H.C. Starck Amperit® 551.059 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
Density
3.70
-
4.40
g/cc
0.134
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
Density
3.70
-
4.40
g/cc
0.134
-
0.159
lb/in³
ASTM B212
H.C. Starck Amperit® 551.088 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)