Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.02 - 2.70 g/cc | 0.0368 - 0.0975 lb/in³ | Average value: 1.14 g/cc Grade Count:328 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #11 Filtration Granule (Corona) 3M #11 Filtration Granules are natural minerals used for water filtration in irrigation system.Information provided by 3M |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #11 Roofing Granule (Corona) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #11 Roofing Granule (Little Rock) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #14 Roofing Granule (Corona) 3M #14 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #18 Roofing Granule (Corona) 3M #18 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M 7000 Series Copper Roofing Granule (Little Rock) 3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Blended #11 Blended Roofing Granule (Little Rock) 3M #11 Grade Blended Roofing Granules are combination of ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Cool Roofing Granule (Corona) 3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products and are designed specifically to have a higher total solar reflectance than standard granu.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Headlap Roofing Granule (Corona) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Headlap Roofing Granule (Little Rock) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Density | 2.65 - 2.70 g/cc | 0.0957 - 0.0975 lb/in³ | |
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |