Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.74 - 2.06 g/cc | 0.0629 - 0.0744 lb/in³ | Average value: 1.83 g/cc Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.95 - 2.06 g/cc | 0.0704 - 0.0744 lb/in³ | ASTM D792 |
Zeus THV Tubing THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity. |
|||
Density | 2.02 - 2.06 g/cc | 0.0730 - 0.0744 lb/in³ | ISO R 1183 |
Fainplast Compounds CRKA 90 Flexible PVC, Flame Retardant Electrical Bedding Lead Free Bedding non contaminating on XLPE |
|||
Density | 0.880 - 2.06 g/cc | 0.0318 - 0.0744 lb/in³ | Average value: 1.37 g/cc Grade Count:1191 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |