Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.70 - 2.00 g/cc | 0.0614 - 0.0723 lb/in³ | Average value: 1.86 g/cc Grade Count:14 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Density | 1.25 - 2.00 g/cc | 0.0452 - 0.0723 lb/in³ | Average value: 1.74 g/cc Grade Count:7 |
Overview of materials for Phenolic/Glass Fiber SMC This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Density | 1.85 - 2.00 g/cc @Temperature 25.0 °C |
0.0668 - 0.0723 lb/in³ @Temperature 77.0 °F |
|
Hong Kun Group APP (Phase II) Flame Retardant |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
Density | 1.60 - 2.00 g/cc | 0.0578 - 0.0723 lb/in³ | Tap |
Solvay CEROXâ„¢ 1650 Surfactant Description: Ceroxâ„¢1650 offers an optimized polishing performance for optical and ophthalmic lenses as well as for other demanding applications like photomask and glass hard disks. Benefits: Hi.. |
|||
Density | 1.60 - 2.00 g/cc | 0.0578 - 0.0723 lb/in³ | Tap |
Solvay SUPER CEROXâ„¢ 1663 Surfactant Description: Super Ceroxâ„¢1663 is particularly suited for the polishing of ophthalmic lenses (mass production and prescription) and optical lenses. Benefits: High polishing efficiency, Very high.. |
|||
Density | 1.96 - 2.00 g/cc | 0.0708 - 0.0723 lb/in³ | ISO R 1183 |
Fainplast Compounds CRA 84 Flexible PVC, Flame Retardant Electrical Bedding Flame retardant bedding |
|||
Density | 1.00 - 2.00 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.0361 - 0.0723 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Palusol® SW 60-1 FSC 100% Silicate Panel Information provided by BASF |
|||
Density | 1.80 - 2.00 g/cc | 0.0650 - 0.0723 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm.. |
|||
Density | 1.80 - 2.00 g/cc | 0.0650 - 0.0723 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion.. |
|||
Density | 1.80 - 2.00 g/cc | 0.0650 - 0.0723 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p.. |
|||
Density | 0.917 - 2.00 g/cc | 0.0331 - 0.0723 lb/in³ | Average value: 0.988 g/cc Grade Count:76 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties... |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer