Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.900 - 1.92 g/cc | 0.0325 - 0.0694 lb/in³ | Average value: 1.31 g/cc Grade Count:184 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Density | 1.66 - 1.92 g/cc | 0.0600 - 0.0694 lb/in³ | Average value: 1.77 g/cc Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Density | 1.88 - 1.92 g/cc | 0.0679 - 0.0694 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 087/2 Halogen Free PVC Filling and bedding |
|||
Density | 1.88 - 1.92 g/cc | 0.0679 - 0.0694 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFC 0115/1 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds |
|||
Density | 1.88 - 1.92 g/cc | 0.0679 - 0.0694 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFC 087/2 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds |
|||
Density | 1.72 - 1.92 g/cc | 0.0621 - 0.0694 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili.. |
|||
Density | 1.72 - 1.92 g/cc | 0.0621 - 0.0694 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |
|||
Density | 1.79 - 1.92 g/cc | 0.0647 - 0.0694 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |