Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.930 - 1.68 g/cc | 0.0336 - 0.0607 lb/in³ | Average value: 1.06 g/cc Grade Count:35 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Density | 1.25 - 1.68 g/cc | 0.0452 - 0.0607 lb/in³ | Average value: 1.53 g/cc Grade Count:41 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Density | 0.920 - 1.68 g/cc | 0.0332 - 0.0607 lb/in³ | Average value: 1.28 g/cc Grade Count:767 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Density | 1.64 - 1.68 g/cc | 0.0592 - 0.0607 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 80/E Flexible PVC, Sheathing Lead Free Under sheathing |
|||
Density | 1.64 - 1.68 g/cc | 0.0592 - 0.0607 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 89/3 Flexible PVC, Flame Retardant Sheathing Sheathing low emission acid fumes |
|||
Density | 1.55 - 1.68 g/cc | 0.0560 - 0.0607 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Density | 1.05 - 1.68 g/cc | 0.0379 - 0.0607 lb/in³ | Average value: 1.31 g/cc Grade Count:46 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |