Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.16 - 1.42 g/cc @Temperature 200 - 215 °C |
0.0419 - 0.0513 lb/in³ @Temperature 392 - 419 °F |
Average value: 1.22 g/cc Grade Count:16 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.26 - 1.42 g/cc | 0.0455 - 0.0513 lb/in³ | Average value: 1.37 g/cc Grade Count:43 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Density | 1.18 - 1.42 g/cc | 0.0426 - 0.0513 lb/in³ | Average value: 1.32 g/cc Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Density | 1.19 - 1.42 g/cc @Temperature 250 - 250 °C |
0.0430 - 0.0513 lb/in³ @Temperature 482 - 482 °F |
Average value: 1.31 g/cc Grade Count:4 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.10 - 1.42 g/cc | 0.0397 - 0.0513 lb/in³ | Average value: 1.26 g/cc Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Density | 1.35 - 1.42 g/cc | 0.0488 - 0.0513 lb/in³ | Average value: 1.38 g/cc Grade Count:4 |
Overview of materials for Nylon 11 with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ.. |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 059/1 Rigid PVC, Injection Molding Fittings high fluidity |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 50 Rigid PVC, Injection Molding Technical items |
|||
Density | 1.34 - 1.42 g/cc | 0.0484 - 0.0513 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Radel® R-7700 Polyphenylsulfone (PPSU) Radel® R-7700 polyphenylsulfone sheet was developed specifically for aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, .. |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 74 Flexible PVC, Sheathing Mineral oil resistent |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 79 Flexible PVC, Insulation Low temperatures |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 63 Flexible PVC, Flame Retardant Sheathing Good flexibility |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 80/R Flexible PVC, Flame Retardant Sheathing Lead Free Minearl oil resistant |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds GS 77 Flexible PVC, Electrical Plugs Plugs |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 77 Flexible PVC, Injection Molding for Technical Items Plugs |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds PMS 96 Flexible PVC, Extrusion Semi-rigid adhesive profiles |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 77 Flexible PVC, Insulation for High Temperatures Lead Free Operating temperature 105°C |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 90/2 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Density | 1.36 - 1.42 g/cc | 0.0491 - 0.0513 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Density | 1.37 - 1.42 g/cc | 0.0495 - 0.0513 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Density | 1.26 - 1.42 g/cc | 0.0455 - 0.0515 lb/in³ | Average value: 1.31 g/cc Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding Electric antishock fittings |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 93 Flexible PVC, Sheathing Lead Free Sheathing automotive cables |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 62 Flexible PVC, Sheathing Sheath various purposes good flexibility |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 88/1 Flexible PVC, Flame Retardant Insulation Lead Free Insulation low temperatures |