Polymer Property : Density = 1.399 g/cc
Polymer Property :
Density =
1.399 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.389
-
1.399
g/cc
0.05018
-
0.05054
lb/in³
M2E-71-065 test
Invista T 94 PET Copolymer Packaging Resin (discontinued **)