Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.24 - 1.29 g/cc @Temperature 250 - 295 °C |
0.0448 - 0.0466 lb/in³ @Temperature 482 - 563 °F |
Average value: 1.26 g/cc Grade Count:7 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Density | 1.05 - 1.29 g/cc | 0.0379 - 0.0466 lb/in³ | Average value: 1.14 g/cc Grade Count:29 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.26 - 1.29 g/cc | 0.0455 - 0.0466 lb/in³ | 309-1D Resin |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Density | 1.21 - 1.29 g/cc | 0.0437 - 0.0466 lb/in³ | OSTM059 |
Solvay TOLCIDE® PS 50A 50% tetrakis hydroxymethyl phosphonium sulfate Identification: PROPRIETARY FORMULATION BASED ON TETRAKIS (HYDROXYMETHYL) PHOSPHONIUM SULPHATE (THPS) BLENDED WITH A NOVEL POLYMERIC PERFORMANCE ENHANCER.Function: Industrial biocidal productBiodegr.. |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 64 Flexible PVC, Sheathing Good flexibility at low temperatures |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 001/AL Flexible PVC, Insulation Lead Free General purposes suitable for food contact according to CEE 90/128 |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7512 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 6020 Flexible PVC, Injection Molding for Footwear High boots |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 6520 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/AS Flexible PVC, Transparent Extrusion Food belt carriers |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75/AS Flexible PVC, Transparent Extrusion Food belt carriers |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds PHS 75/B Flexible PVC, Transparent Extrusion Pipes for gasoline CAVIS |
|||
Density | 1.03 - 1.29 g/cc | 0.0372 - 0.0466 lb/in³ | Average value: 1.13 g/cc Grade Count:91 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.12 - 1.29 g/cc | 0.0405 - 0.0466 lb/in³ | Average value: 1.19 g/cc Grade Count:26 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |