Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.21 - 1.222 g/cc | 0.0437 - 0.04415 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DX99620C PC LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |