Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.125 - 1.145 g/cc | 0.04064 - 0.04137 lb/in³ | AV15 |
Solvay Butyl Acid Phosphate Identification: Di(n-butyl) phosphoric acid: 45 – 50% and n-Butyl phosphoric acid: 45 – 50%CAS: 1623-15-0; 107-66-4Available in: Asia Pacific, Europe, Latin America and North AmericaAppli.. |
|||
Density | 1.05 - 1.145 g/cc | 0.0379 - 0.04137 lb/in³ | |
Solvay RHODOLINE® 111 Surfactant Description: Hydrophobic copolymer dispersant. Highly versatile, flat to gloss, interior/exterior, low foam, excellent water resistanceIdentification: AQUEOUS SOLUTION OF POLY CARBOXYLIC ACID SALT A.. |