Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.079 - 1.099 g/cc | 0.03898 - 0.03970 lb/in³ | ASTM D4052 |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |