Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.937 - 0.945 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez 298-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.937 - 0.945 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez 298-285D High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.913 - 0.945 g/cc | 0.0330 - 0.0341 lb/in³ | Average value: 0.935 g/cc Grade Count:49 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Density | 0.924 - 0.945 g/cc | 0.0334 - 0.0341 lb/in³ | Average value: 0.937 g/cc Grade Count:67 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i.. |
|||
Density | 0.927 - 0.945 g/cc | 0.0335 - 0.0341 lb/in³ | Average value: 0.939 g/cc Grade Count:17 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |