Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Density | 0.921 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Density | 0.920 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.920 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4222M (224F7) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Density | 0.9185 - 0.924 g/cc | 0.03318 - 0.0334 lb/in³ | |
Kazanorgsintez 102-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Density | 0.9185 - 0.924 g/cc | 0.03318 - 0.0334 lb/in³ | |
Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-15 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-16 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-17 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-21 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-23 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 107-18 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 107-19 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 107-20 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 107-22 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.9185 - 0.924 g/cc | 0.03318 - 0.0334 lb/in³ | |
Kazanorgsintez 153-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Density | 0.9185 - 0.924 g/cc | 0.03318 - 0.0334 lb/in³ | |
Kazanorgsintez 153-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-15 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-21 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-23 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-17 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-16 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |