Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.820 - 0.880 g/cc | 0.0296 - 0.0318 lb/in³ | fired density (compressed) |
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Density | 0.820 - 0.880 g/cc | 0.0296 - 0.0318 lb/in³ | fired density (compressed) |
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |