Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.839 - 0.869 g/cc | 0.0303 - 0.0314 lb/in³ | |
Lord Adhesives Chemlok® Y-1540 Silicone Rubber Adhesive Chemlok® Y-1540 is a one-coat adhesive used to bond peroxide curing silicone, EPDM, and fluoroelastomers to cold rolled and phosphatized steel.All information provided by Lord. |