Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.368 - 0.481 g/cc @Treatment Temp. 982 °C, Time 86400 sec |
0.0133 - 0.0174 lb/in³ @Treatment Temp. 1800 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® Isofoam® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Density | 0.368 - 0.481 g/cc @Treatment Temp. 982 °C, Time 86400 sec |
0.0133 - 0.0174 lb/in³ @Treatment Temp. 1800 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Density | 0.368 - 0.481 g/cc @Treatment Temp. 1260 °C, Time 86400 sec |
0.0133 - 0.0174 lb/in³ @Treatment Temp. 2300 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® RG Plus Insulation Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process.. |
|||
Density | 0.417 - 0.481 g/cc | 0.0150 - 0.0174 lb/in³ | |
Engineered Syntactic Systems BZ-28 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |